Atomic Layer Deposition of Tin Monosulfide Thin Films

Title Atomic Layer Deposition of Tin Monosulfide Thin Films
Author: Sinsermsuksakul, Prasert; Heo, Jaeyeong; Noh, Wontae; Hock, Adam S. & Gordon, Roy G.
Advanced Energy Materials, November 2011
2011
http://doi.wiley.com/10.1002/aenm.201100330
More details: Thin film solar cells made from earth-abundant, non-toxic materials are needed to replace the current technology that uses Cu(In,Ga)(S,Se) 2 and CdTe, which contain scarce and toxic elements. One promising candidate absorber material is tin monosulfide (SnS). In this report, pure, stoichiometric, singlephase SnS films were obtained by atomic layer deposition (ALD) using the reaction of bis( N, N?�?- diisopropylacetamidinato)tin(II) [Sn(MeC(N- i Pr) 2) 2] and hydrogen sulfide (H 2S) at low temperatures (100 to 200 ??C). The direct optical band gap of SnS is around 1.3 eV and strong optical absorption ($\alpha$\>10 4cm - 1 ) is observed throughout the visible and near-infrared spectral regions. The films are p-type semiconductors with carrier concentration on the order of 10 16cm -3 and hole mobility 0.82-15.3 cm 2 V -1 s -1 in the plane of the films. The electrical properties are anisotropic, with three times higher mobility in the direction through the film, compared to the in-plane direction. ?? 2011 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
ISBN1614-6840

No comments:

Post a Comment